Title:Behavior of ultra-low temperature medium bulging for aluminum alloy tube
Authors: Fan Xiaobo Wang Xugang Chen Xianshuo Yuan Shijian 
Unit: Dalian University of Technology Harbin Institute of Technology 
KeyWords: aluminum alloy special-shaped tube  ultra-low temperature medium bulging  bulging performance  deformation uniformity 
ClassificationCode:TG394
year,vol(issue):pagenumber:2021,46(4):1-5
Abstract:

For the problem of easy cracking for aluminum alloy complex special-shaped tube, an ultra-low temperature medium bulging method was proposed by the double-increasing effect of simultaneous increase of elongation and hardening index for aluminum alloy at ultra-low temperature, and the bulging performance of 6061 aluminum alloy tube under the condition of liquid nitrogen temperature (-196 ℃) was tested by establishing the device of ultra-low temperature medium bulging for tube. Then, the corresponding free bulging behavior of aluminum alloy tube at ultra-low temperature was analyzed by experiment and FEM. The results show that the bulging performance of aluminum alloy tube is significantly improved under ultra-low temperature condition (-196 ℃), and the expansion rate is increased from 17.4% at normal temperature to 34.5% which is increased by nearly onetime. Furthermore, the hardening ability of aluminum alloy tube at ultra-low temperature is also enhanced, and the deformation is more uniform. At the same deformation stage, the ultimate strain and strain gradient of free bulging deformation zone are gradually reduced with the increasing of hardening index value of n.
 

Funds:
国家重点研发计划项目(2019YFA0708804);中央高校基本科研业务费专项资金资助(DUT20ZD101)
AuthorIntro:
凡晓波(1987-),男,博士,副研究员 E-mail:xbfan@dlut.edu.cn
Reference:


[1]Yuan S J, Fan X B. Developments and perspectives on the precision forming processes for ultra-large size integrated components
[J]. International Journal of Extreme Manufacturing, 2019,1: 1-18.



[2]刘勇,耿会程,朱彬,等. 高强铝合金高效热冲压工艺研究进展
[J].锻压技术,2020,45(7):1-12.


Liu Y, Geng H C, Zhu B, et al. Research progress on high efficiency hot stamping process for high strength aluminum alloy
[J]. Forging & Stamping Technology, 2020,45(7):1-12.



[3]Dursun T, Soutis C. Recent developments in advanced aircraft aluminium alloys
[J]. Materials & Design, 2014, 56: 862-871.



[4]Manabe K, Fuchizawa S. Further development on tube hydroforming
[J]. 60 Excellent Inventions in Metal Forming, 2015,4:387-393.



[5]Lee M G, Korkolis Y P, Kim J H. Recent developments in hydroforming technology
[J]. Proc.IMechE, Part B: J.Engineering Manufacture, 2015, 229(4): 572-596.



[6]KoM. Hydroforming for Advanced Manufacturing
[M]. Cambridge:Woodhead Publishing,2008.



[7]Hirsch J. Recent development in aluminium for automotive applications
[J]. Transactions of Nonferrous Metals Society of China, 2014, 24(7): 1995-2002.



[8]Zheng K L, Politis D J, Wang L L, et al. A review on forming techniques for manufacturing lightweight complexdshaped aluminium panel components
[J]. International Journal of Lightweight Materials and Manufacture, 2018,1: 55-80.



[9]Cai Y, Wang X S, Yuan S J. Analysis of surface roughening behavior of 6063 aluminum alloy by tensile testing of a trapezoidal uniaxial specimen
[J]. Materials Science and Engineering: A, 2016, 672: 184-193.



[10]束飞,拓建峰,张宇岑,等. 飞机铝合金深锥型面零件多道次充液拉深技术
[J].精密成形工程,2016,8(5):96-102.


Shu F, Tuo J F, Zhang Y C, et al. Multi-step hydrodynamic deep drawing of aluminium alloy conical part with deep cavity
[J]. Journal of Netshape Forming Engineering, 2016,8(5):96-102.



[11]刘晓滕,赵佳蕾,孙有政,等. 中间退火对Al-Mg-Si系铝合金汽车板组织和性能的影响
[J].金属热处理,2020,45(10):119-124.


Liu X T, Zhao J L, Sun Y Z, et al. Effect of intermediate annealing on microstructure and properties of Al-Mg-Si series aluminum alloy automobile sheet
[J]. Heat Treatment of Metals, 2020,45(10):119-124.


[12]Cheng W J, Liu W, Yuan S J. Deformation behavior of Al-Cu-Mn alloy sheets under biaxial stress at cryogenic temperatures
[J]. Materials Science and Engineering: A, 2019, 759:357-367.



[13]陈鼎,陈振华. 铝合金在低温下的力学性能
[J]. 宇航材料工艺, 2000,(4):1-7.


Chen D, Chen Z H. Mechanical properties of pure aluminum alloys at cryogenic temperatures
[J]. Aerospace Materials & Technology, 2000,(4):1-7.



[14]Cheng W J, Liu W, Fan X B, et al. Cooperative enhancements in ductility and strain hardening of a solution-treated Al-Cu-Mn alloy at cryogenic temperatures
[J]. Materials Science and Engineering: A, 2020, 790:1-14.

 

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com