Title:Investigation on deformation characteristics of internal spinning incremental forming process for metal corrugated tubes
Authors: Shi Xun  Li Yan  Yang Mingshun  Yao Zimeng  Hou Xiaoli  Yuan Qilong  Jiang Feilong 
Unit: Xi′an University of Technology 
KeyWords: spinning  incremental forming  metal corrugated tubes material deformation  ABAQUS/Explicit 
ClassificationCode:TG376.9
year,vol(issue):pagenumber:2018,43(2):0-0
Abstract:

 The internal spinning incremental forming technology for metal corrugated tubes was carried out by combining incremental forming technology with tube spinning forming process. Then, the finite element model of internal spinning incremental forming for metal corrugated tubes based on ABAQUS/Explicit was established in order to obtain the change rules of material in the forming region, and the thickness reduction and torsional variation of material were analyzed in the forming process. Furthermore, the experimental platform of internal spinning incremental forming for metal corrugated tubes was built, the experiments of incremental forming for metal corrugated tube were conducted, and the thickness variation of tube wall in the forming region was measured and analyzed along the thickness direction,which verified the correctness of the finite element numerical model and the theoretical calculation results. Finally, the experiment of incremental forming multi corrugations was repeated to verify the reliability of forming process. Thus, the change rules of surface microstructure for tube wall in deformation region shows that the plastic strain of material in the transition region of arc and the tensile region of inclined plane is large, in which the tube wall is prone to produce excessive deformation and crack,and then the forming quality and precision of tube are affected.

Funds:
国家自然科学基金资助项目(51475366,51475146)
AuthorIntro:
作者简介:石珣(1990-),男,硕士研究生 E-mail:18109234315@163.com 通讯作者:李言(1960-),男,博士,教授,博士生导师 E-mail:18729380286@163.com
Reference:

 
[1]Behera A K, Sousa R A D, Ingarao G, et al. Single point incremental forming: An assessment of the progress and technology trends from 2005 to 2015
[J]. Journal of Manufacturing Processes, 2017, 27:37-62. 


 


[2]Yang H, Li H, Zhang Z Y, et al. Advances and trends on tube bending forming technologies
[J]. Chinese Journal of Aeronautics, 2012, 25(1):1-12.

 


[3]Mei Z, Guo K, Yang H. Advances and trends in plastic forming technologies for welded tubes
[J]. Chinese Journal of Aeronautics, 2016, 29(2):305-315.

 


[4]Teramae T, Manabe K, Ueno K, et al. Effect of material properties on deformation behavior in incremental tube-burring process using a bar tool
[J]. Journal of Materials Processing Technology, 2007, 191(1):24-29.

 


[5]Becker C, Tekkaya A E, Kleiner M. Fundamentals of the incremental tube forming process
[J]. CIRP Annals-manufacturing Technology, 2014, 63(1):253-256.

 


[6]Raujol-Veillé J, Toussaint F, Tabourot L, et al. Experimental and numerical investigation of a short, thin-walled steel tube incremental forming process
[J]. Journal of Manufacturing Processes, 2015, 19:59-66.

 


[7]Alves M L, Almeida B P P, Rosa P A R, et al. End forming of thin-walled tubes
[J]. Journal of Materials Processing Technology, 2006, 177(1-3):183-187.

 


[8]Farahmand H R, Abrinia K. An upper bound analysis for reshaping thick tubes to polygonal cross-section tubes through multistage roll forming process
[J]. International Journal of Mechanical Sciences, 2015, 100:90-98.

 


[9]Negendank M, Müller S, Reimers W. Extrusion of aluminum tubes with axially graded wall thickness and mechanical characterization
[J]. Procedia Cirp., 2014, 18(18):3-8.

 


[10]鲁素玲,李军,张双杰,等.厚壁管开式冷挤压坯料集合逆向预测研究
[J].机械工程学报,2014,50(10):98-102.

 

Lu S L, Li J, Zhang S J, et al. Reverse prediction studies of billets set on open-die cold extrusion of thick wall pipe
[J]. Journal of Mechanical Engineering, 2014, 50(10):98-102.

 


[11]夏琴香.三维非轴对称零件旋压成形机理研究
[J].机械工程学报,2004,40(2):153-156.

 

Xia Q X. Investigation on the mechanism of the spinning technology of the 3D non-axisymmetric parts
[J]. Journal of Mechanical Engineering, 2004, 40(2):153-156.

 


[12]Salem E, Shin J, Nath M, et al. Investigation of thickness variation in single point incremental forming
[J]. Procedia Manufacturing, 2016, 5:828-837.

 


[13]Oleksik V. Influence of geometrical parameters, wall angle and part shape on thickness reduction of single point incremental forming
[J]. Procedia Engineering, 2014, 81:2280-2285.

 


[14]周六如.板料数控渐进成形变形区厚度变化规律的研究
[J].机械工程学报,2011,47(18):50-54.

 

Zhou L R. Research on the thickness change laws in numerical control incremental sheet forming
[J]. Journal of Mechanical Engineering, 2011, 47(18):50-54.

 


[15]曹宇,高锦张,贾俐俐,等.渐进成形圆孔翻边变形区厚度减薄现象的模拟研究
[J].锻压技术, 2015,40(2):52-59.

 

Cao Y, Gao J Z, Jia L L, et al. Numerical simulation for thickness thinning of deformation zone on hole-flanging by incremental forming
[J]. Forging & Stamping Technology, 2015, 40(2):52-59.
Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com