Title:Research on technological parameters of hydroforming for titanium T-shaped tube
Authors: Zhu Mingqing Ji Weixi Zhang Xu Jia Jiyong 
Unit: Jiangnan University Wuxi Xinfeng Pipe-Fittings Corp. 
KeyWords: titanium T-shaped tube hydroforming FEM simulation 
ClassificationCode:
year,vol(issue):pagenumber:2015,40(1):56-60
Abstract:

The hydroforming process of Φ219 mm×Φ219 mm×5 mm titanium T-shaped tube was studied by Dynaform. With the effective height of branch pipe, the biggest thinning ratio and the biggest thickening rate as optimization criterion, an optimal scheme was obtained by calculating various combinations of technological parameters including loading paths of the internal pressure, pressure duration, velocities on left, right and middle of the punch etc. Finally a practical hydroforming experiment was conducted according to the technological parameters of the optimal scheme. The research indicates that the third scheme has the best forming effect, and the effective height of branch pipe is 68.41mm, with the biggest thinning ratio and thickening rate are 27.38% and 54.34% respectively. The requirements on the size and wall thickness distribution of T-shape tube are met. Compared with the simulation results, the errors of effective height of branch pipe, the biggest thinning ratio and the biggest thickening rate from the experiment are all less than 5.1%.
 

Funds:
江苏省“六大人才高峰”资助项目(2010-JXQC-089)
AuthorIntro:
朱明清(1990-),男,硕士研究生
Reference:


[1]彭剑,周昌玉,代巧,等. 工业纯钛室温下的应变速率敏感性及Hollomon经验公式的改进[J] . 稀有金属材料与工程,2013,42(3):483-487.Peng J,Zhou C Y,Dai Q,et al. Strain rate sensitivity of commercially pure titanium TA2 at room temperature and revising of hollomon empirical formula[J].Rare Metal Meterials and Engineering,2013,42(3):483-487.



[2]张永强,胡伟民,赵国超,等 . 钛合金无缝T型管件液压胀形[J] . 锻压技术,2010,35(1):63-65.Zhang Y Q,Hu W M,Zhao G C,et al.Hydraulic bulging of titanium alloy seamless T-type tube fittings[J].Forging & Stamping Technology,2010,35(1):63-65.



[3]郭训忠,陶 杰,李 鸣 . 模具型面及冲头对304不锈钢三通成形效果影响研究[J] . 中国机械工程,2010,21(15):1875-1878.Guo X Z,Tao J,Li M. Influence of die surface and punch style on forming effects of SS304 T-Shapes by hydrogforming[J].China Mechanical Engineering,2010,21(15):1875-1878.



[4]郭训忠,陶杰,刘红兵,等 . 聚变堆用难变形CLAM钢三通成形模拟及试验研究[J]. 原子能科学技术,2010,44(10):1217-1222.Guo X Z,Tao J,Liu H B,et al. Numerical simulation and experimental study of CLAM T-shapes for fusion applications by hydroforming[J]. Atomic Energy Science and Technology,2010,44(10):1217-1222.



[5]苑世剑,王小松 . 液压成形技术研究与应用新进展[J] . 塑性工程学报,2008,15(2):22-30.Yuan S J,Wang X S. Developments in researches and applications of tube hydroforming[J].Journal of Plasticity Engineering,2008,15(2):22-30.



[6]Teng B G,Yuan S J,Chen Z T,et al. Plastic damage of T-shape hydroforming[J]. Transactions of Nonferrous Metals Society of China,2012,(22):294-301.



[7]Giuseppe Ingarao,Rosa Di Lorenzo,Fabrizio Micari . Internal pressure and counterpunch action design in Y-shaped tube hydroforming processes: A multi-objective optimization approach[J]. Computers & Structures,2009,87:591-602.



[8]Teng B G,Li K,Yuan S J. Optimization of loading path in hydroforming T-shape using fuzzy control algorithm[J]. Int. J. Adv .Manuf. Technol.,2013,69:1079-1086.



[9]王鑫,余心宏. Y型三通管内高压成形机理及补料比的影响研究[J].材料工程,2013,(1):35-39.Wang X,Yu X H. Hydroforming mechanism of Y-shaped tube and influence of axial feed ratio on forming[J]. Journal of Materials Engineering,2013,(1):35-39.



[10]Kadkhodayan M, Erfani-Moghadam A . An investigation of the optimal load paths for the hydroforming of T-shaped tubes[J].Int.J .Adv. Manuf. Technol.,2012,61:73-85.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com