Title:Prediction of cylinder re-drawing performance
Authors: ZHOU Xiao-hong 
Unit: Chinese Academy of Sciences 
KeyWords: limiting drawing ratio redrawing conical die bending 
ClassificationCode:TG113.26
year,vol(issue):pagenumber:2010,35(5):52-55
Abstract:

An equation was established to predict the limiting redrawing ratio of cylinder cup, which was based on the redrawing process, using slab method, friction theory and sheet bending/unbending theory around the die arc radius.  Commercially pure titanium (TA1) cups were used for deep drawing experiments, and the effects of various parameters, such as average normal anisotropy 〖AKR-〗, friction coefficient μ, half die cone anger α, radius of the die arc rd, cup thickness ration tmax/tmin on redrawing were discussed.  The results show that the calculation from the model is in good agreement with the experimental results by the experiments, and the limiting redrawing ratio increases linearly with R, but decreases almost linearly with μ and tmax/tmin.

Funds:
AuthorIntro:
Reference:


[1]Whiteley R L. The importance of directionality in drawing quality sheet steel [J]. Trans. ASM.,1960, 52: 154-163.
[2]Mir W A, Hillier M J. Cup drawing from an anisotropic blank [J]. J. Eng. Ind. Trans. ASME.,1969, 89: 766-771.
[3]Shawki G S A. Assessing deep-drawing qualities of sheet metal[J]. Sheet Met. Ind.,1965,42: 417-424 .
[4]Akamatsu T, Ukita S, Miyasaka K,et al. Deep drawing of commercially pure titanium sheets [J]. ISIJ Int.,1995, 35: 56-62.
[5]Leu D K. The limiting drawing ratio for plastic instability of the cup-drawing process[J]. J. Mater. Process. Technol.,1999, 86: 168-176.
[6]Verma R K, Chandra S. An improved model for predicting limiting drawing ratio[J]. J. Mater. Process. Technol.,2006, 172: 218-224.
[7]陆文琼,陈劫实,陈军. 一种板料拉深性能的快捷解析预测方法[J].锻压技术, 2009, 34(2): 67-70.
[8]刘建华,王志恒. 平面压边拉深工艺参数对内皱影响及试验研究[J]. 锻压技术, 2008, 33(2): 50-53.
[9]杨建华,潘伟,何丹农,等. 板料多道次拉深成形规律和性能的研究[J]. 锻压技术, 2005, 30(5): 22-24.
[10]Hill R. The mathematical theory of plasticity[M]. Oxford: Clarendon Press, 1950.
[11]萧弗曼.冷压原理[M].北京:机械工业出版社,1957.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com