Abstract:
|
The inner-wrinkle is easy to be produced at the suspending zone during drawing the curved surface parts.Increasing the holder force can avoid the inner-wrinkle,and the critical holder force is decided by some processing parameters.According to the deformation of drawing under blank holder,critical calculation for innere-wrinkle was carried out,and the checking condition for drawing cone and sphericity parts were gained.Then,the effect of main parameters on inner-wrinkle was studied by experiment for drawing cone parts,such as material characteristics,relative thickness,drawing coefficient and so on.The results show that decreasing material hardenability value,radius ratio of punch-die and the relative thickness,the trend of inner-wrinkle is increased;but reducing drawing coefficient,the inner-wrinkle is postponed.Therefore,reasonably selecting the processing parameters shall avoid the inner-wrinkle during drawing curved surface parts.
|
Funds:
|
长安大学青年科学基金(06Z11)
|
AuthorIntro:
|
|
Reference:
|
[1]徐尚德,雷君相,于珊珊.板料拉深过程中的压边力控制技术[J].锻压装备与制造技术,2004,(2),51-55.
[2]赵军,马瑞,官英平,等.锥形件拉深智能化控制中压边力的控制规律[J].材料科学与工艺,2004,12(4):439-441,445.
[3]王作成,韩福涛,崔国涛.圆锥形件变压边力拉深工艺的研究[J].塑性工程学报,2006,13(2):25-28.
[4]陶友瑞,张福全,黄长青.半球形件冲压成形的防内皱压边力研究[J].塑性工程学报,2004,11(1):29-31.
[5]孙成智,罗思东,王东川,等.拉深过程中压边力分布实验测量方法与数值模拟[J].锻压技术,2005,30(6):18-21.
[6]刘建华,丁国,王志恒.内皱发生的临界计算及校核条件[J].锻压技术,2000,25(2):8-31.
[7]梁炳文,胡世光.板料成形塑性理论[M].北京:机械工业出版社,1987.
[8]王孝培.冲压手册[M].北京:机械工业出版社,1988.
|
Service:
|
【This site has not yet opened Download Service】【Add
Favorite】
|
|
|