Abstract:
|
The shape of rear cover outer top is very complicated,and there are many local features. The stamping process is of six operations. During try-out,serious wrinkle had occurred in the fifth operation,which would damage surface quality and result in bad weldable. It was found that unreasonable restrike process is the main causation. Therefor,the restrike CAM was improved. First,a small pad was added. Second,material absorbing groove was added on the surface. Then,the structure of restrike block was re-designed. By means of these methods,wrinkle was ultimately eliminated and part's quality was evidently improved.
|